- Sand cast casting
- Investment kukanda
- Die Kudzingwa
- Low kumanikidzwa Kudzingwa
- Centrifugal kukanda
- Giravhiti Kufa Kukanda
- Vacuum Kudzingwa
- Dzvanya kukanda
- Yakarasika furo kukanda
- Kuenderera mberi kwekukanda
1.Sand Kukanda
Kukanda jecha: Nzira yekukanda yekuburitsa castings mujecha. Simbi, simbi uye yakawanda isiri-ferrous chiwanikwa castings inogona kuwanikwa nejecha kukanda nzira.
Maitiro kuyerera:
- a: Kugadzira Mould Mharidzo
- b: Kugadzirira Kwekugadzira Sand
- c: yakanyungudutswa simbi
- d: Kugadzira Core Sand
- e: Kugadzira Core Bhokisi
- ini: Wet Rudzi
- j: Rakaoma Rudzi
- f1: Kugadzira Jecha
- g1: Kuomesa Jecha
- f2: Kugadzira Sand Core
- g2: Kuomesa Sand Core
- h: Iyo Mforoma Inoumbwa SeMold
- k: Tora Kunze Kukanda Kubva muforoma
- m: Chenesa Up
- n: Kuongorora Zvikamu
Technical Features:
- Iyo inokodzera kugadzira mabhureki ane akaomarara maumbirwo, kunyanya ane akaomesesa emukati mhango;
- Wide inochinjika uye yakaderera mutengo;
- Kune zvimwe zvinhu zvine mashoma mapurasitiki, senge simbi yakakandwa, kukandwa kwejecha ndiyo chete nzira yekuumba yekugadzira zvikamu zvaro kana zvisipo.
- Kushanda: mota injini cylinder block, cylinder musoro, crankshaft uye mamwe ma castings
2.Investment Kukanda
Investment casting: inowanzoreva kugadzira pateni yakagadzirwa nefusible materials, ichifukidza pamusoro peiyo pateni nematanho akati wandei ezvigadziriso zvinhu kuti vagadzire goko, uye vozonyungudza pateni kubva mugobvu kuti vatore furemu isina nzvimbo yekuparadzanisa. Mushure mekushisa kwepamusoro kubheka Ipapo, inogona kuzadzwa nejecha ndokudururwa. Kazhinji zvinonzi "wakarasa wakisi kukanda".
- a: muforoma Kugadzira
- b: Kukanda Dhayagiramu
- c: Kusvuta
- d: Kuongorora kwechikamu
- e: Kunhonga Passivation
- f1: Wax Jekiseni
- f2: Wax Muenzaniso
- f3: Welding Kudira Riser
- f4: Pendi Yakarembera
- f5: Jecha Rakasununguka
- f6: Kuomesa
- f7: Kushushikana
- f8: Mould Shell Kubheka
- f9: Kukanda
- f10: Kukanda
- f11: Chenesa Up
- f12: Kurapa kwekupisa
- f13: Kuongorora
- f14: Kuchengeta
- g: Cnc machine
- h: Kuongorora kwezvikamu
- ini: Warehousing
- j: Wax Yakagadziriswa
- k: Wakisi
Maitiro ehunhu
mukana:
- Kukwirira kwepamusoro uye kujeka kwejometri;
- Yakakwirira yepamusoro roughness;
- Iyo inogona kukanda yakaoma castings, uye iyo cast alloy haina kuganhurirwa.
Kukanganisa: maitiro akaomarara uye mutengo wakakwira
Kunyorera: Inokodzera kugadzirwa kwezvidiki zvidiki zvine maumbirwo akaomarara, yakanyanya kunyatsoita zvinodiwa, kana zvimwe zvinetswa zvekugadzirisa, senge turbine injini mashizha.
3.Kufa Kukanda
Kufa uchikanda: Inoshandisa kumanikidza kwakanyanya kudzvanya simbi yakanyungudutswa kuita chaiyo simbi muforoma mhango pakumhanya. Iyo simbi yakanyungudutswa inotonhorera uye inosimbiswa pasi pekumanikidzwa kuti iite kukanda.
Kufa Kukanda Maitiro:
- Chenesa muforoma
- Tsvina pepa
- Clamping
- Kudurura
- solidify
- Mold
- Eject
- Bvisa kukanda
Maitiro ehunhu
mukana:
- Iyo simbi yemvura inotakura yakanyanya kumanikidza panguva yekufa-kukanda, uye kuyerera chiyero kuri kukurumidza
- Iyo mhando yechigadzirwa yakanaka, saizi yakagadzikana, uye kuchinjika kwakanaka;
- Kugadzira kunyatsoshanda kwakakwirira, uye iyo yekufa-ichikanda muforoma inoshandiswa kakawanda;
- Iyo inokodzera kugadzirwa kwemazhinji nezvakanaka zvehupfumi.
payakaipira:
- Kukanda kunoitika kune madiki pores uye shrinkage porosity.
- Kufa kwekukanda kune yakaderera plastiki uye haina kukodzera kushanda pasi pekukanganisa mutoro uye vibration;
- Kana yakanyanya kusungunuka poindi chiwanikwa chiri kufa-kukanda, hupenyu hwehuvhu hwakadzika, izvo zvinokanganisa kuwedzera kwekufa-kukanda kugadzirwa.
Kushanda: Die castings yakatanga kushandiswa muindasitiri yemotokari uye indasitiri yezviridzwa, uye gare gare yakawedzera kusvika kumaindasitiri akasiyana siyana, senge michina yekurima, muchina wekushandisa indasitiri, indasitiri yemagetsi, indasitiri yezvidziviriro, komputa, zvishandiso zvekurapa, wachi, makamera, uye zvemazuva ese zvigadzirwa. , nezvimwewo.
4.Low Pressure Kukanda
Yakadzvanywa kumanikidzwa kukanda: inoreva nzira yekuzadza chakuvhuvhu nesimbi yemvura pasi pezasi kumanikidza (0.02 ~ 0.06MPa) uye ichidzvinyirira pasi pekumanikidzwa kuti iite castings.
Unyanzvi zvikamu:
- Iko kumanikidza uye nekumhanyisa panguva yekudira zvinogona kugadziridzwa, saka zvinogona kushandiswa kune akasiyana makanda ekuumbika (senge simbi kuumbwa, jecha kuumbwa, nezvimwewo), kukanda akasiyana alloys uye castings eakasiyana saizi;
- Pazasi jekiseni mhando yekuzadza inogamuchirwa, kuzadzwa kwesimbi yakanyungudutswa yakatsiga uye hapana chekupaza chinoitika, icho chinogona kudzivirira kupinda mukati kwegasi uye kukoromoka kwemadziro uye musimboti, izvo zvinovandudza muyero wekupasa kwekukanda;
- Kukanda kunojekesa pasi pekumanikidzwa, chimiro chekukanda chakakora, pepa rejekerere rakajeka, pamusoro pacho panotsvedzerera, uye michina zvivakwa zvakakwirira, izvo zvinonyanya kubatsira kurasa kwakakura uye kwakaonda-kwakakomberedzwa zvikamu;
- Iyo inosimudza inosimudza yasiyiwa, uye iyo simbi yekushandisa mwero inowedzerwa kusvika 90-98%;
- Yakaderera basa kusimba, mashandiro akanaka ezvinhu, zvishandiso zviri nyore, nyore kuona michina uye otomatiki.
Kushanda: Zvikuru zvigadzirwa zvechinyakare (humburumbira musoro, vhiri hub, humburumbira furemu, nezvimwewo).
5.Centrifugal Kukanda
Centrifugal kurasa: inzira yekurasa iyo simbi yakanyungudutswa inodururwa muforoma inotenderera, uye chakuvhuvhu chinozadzwa pasi pechiito chesimba re centrifugal kusimbisa uye kuumbika.
Maitiro ehunhu
mukana:
- Iko kunenge kusisina kushandiswa kwesimbi mune yegeji sisitimu uye iyo riser system, iyo inovandudza mwero wekugadzira weichi chiitiko;
- Izvo hazvidikanwe kushandisa musimboti kana uchigadzira zvisikwa zvisina kukwana, saka simbi yekuzadza kugona inogona kuvandudzwa zvakanyanya kana uchigadzira marefu tubular castings;
- Kukanda kune kwakanyanya kuwanda, mashoma akaremara senge pores uye slag inclusions, uye yakakwira michina zvivakwa;
- Izvo zviri nyore kugadzira dhiramu uye sleeve rinoumbwa nesimbi castings.
payakaipira:
- Iko kune zvimwe zvipingamupinyi kana zvichishandiswa mukugadzirwa kweakakosha-akaumbwa castings;
- Iyo dhayamita yemukati gomba rekukanda haina kukodzera, pamusoro pegomba remukati riine hukasha, mhando iri murombo, uye iyo machining mvumo yakakura;
- Kukanda kunoitika kusarura kweimwe giravhiti.
shanduro:
Kukanda kweCentrifugal kwakatanga kushandiswa mukugadzira pombi dzesimbi. Kumba nekune dzimwe nyika, kukanda kwema centrifugal kwaishandiswa mukugadzira simbi, kuchera, kutakura, kudiridzira uye michina yemadhiraini, avhiyesheni, dziviriro yenyika, mota uye mamwe maindasitiri kugadzira simbi, simbi uye isina-ferrous kabhoni chiwanikwa castings. Pakati pavo, kugadzirwa kweanokanda senge centrifugal cast iron pombi, yemukati injini injini humburumbira liners uye shaft sleeve ndizvo zvakajairika.
6.Gravity Kufa Kukanda
Giravhiti Kufa Kukanda: zvinoreva nzira yekuumba iyo simbi yemvura yakazadzwa neforoma yesimbi pasi pechiitiko chegiravhiti uye yakatonhora uye yakasimbiswa muforoma kuti uwane kukanda.
Maitiro ehunhu
mukana:
- Iyo yekudziya conductivity uye kupisa kugona kwesimbi muforoma zvakakura, iyo inotonhorera mwero inokasira, chimiro chekukanda chakakora, uye michina zvivakwa ingangoita 15% yakakwira kupfuura iyo yejecha kukanda.
- Kukanda neakakwirira epamusorosoro kunyatsoita uye kwakadzika kwepamusoro kukwirisa kukosha kunogona kuwanikwa, uye iko kugadzikana kwemhando kwakanaka.
- Nekuti macores ejecha haashandiswe uye haawanzoshandiswa, nharaunda inovandudzwa, guruva nemagasi anokuvadza anoderedzwa, uye simba revashandi rakadzikira.
payakaipira:
- Iyo simbi muforoma pachayo haina mweya inokwenenzverwa, uye mamwe matanho anofanirwa kutorwa kuti uwane mweya mune iyo mhango uye gasi rinogadzirwa nejecha musimboti;
- Iyo simbi muforoma haina yekudzokera, uye iyo kurasa inowanzo tenderera kutsemuka kana yakasimbiswa;
- Iyo simbi muforoma yekugadzira kutenderera yakareba uye mutengo wakakwira. Naizvozvo, chete mukugadzira kwakawanda, inogona kuratidza mhedzisiro yakanaka yezvehupfumi.
Kushanda: Simbi yekuumbwa simbi haina kukodzera chete kugadzirwa kwemazhinji eisina-ferrous alloy castings senge aluminium alloys uye magnesium alloys ane maitiro akaomarara, asiwo akakodzera kugadzirwa kwesimbi nesimbi simbi castings uye ingots.
7.Vacuum Die Kukanda
Vacuum vachikanda: An yemhando vanofa-vachikanda muitiro kuti anobvisa kana yekudyidzana kunoderedza pores uye ichiputswa magasi ari kufa-vachikanda zvikamu nokubvisa gasi kubva vanofa-vachikanda muforoma mhango panguva kufa-vachikanda muitiro, nokudaro kuvandudza zvemaziso ehupfumi uye pamusoro mhando yezvikamu zvekufa-zvekukanda.
Maitiro ehunhu
mukana:
- Bvisa kana kudzikisa pores mukati mekufa uchikanda, kugadzirisa michina zvivakwa uye pamusoro pehunhu hweanofa kukanda, uye kugadzirisa mashandiro anoita;
- Kuti kuderedze iko kumashure kumanikidzwa kweiyo mhango, kudzikisa yakatarwa kumanikidza uye maalloys ane mashoma ekurasa zvinhu anogona kushandiswa, uye zvinokwanisika kufa-kukanda kwakakura castings nemudiki muchina;
- Iyo yekuzadza mamiriro akavandudzwa, uye vatete vatambi vanogona kufa-kukandwa;
payakaipira:
- Chimiro chekuisa chisimbiso chimiro chakaomarara, uye zvinonetsa kugadzira nekuisa, saka mutengo wakakwira;
- Kana iyo yekufa-yekurasa-nzira yekukanda isina kudzorwa zvakanaka, mhedzisiro haina kunyanya kukosha.
8.Kusvina Die Kukanda
Dzvinya kukanda: inzira yekusimbisa, kuyerera nekuumba simbi kana simbi yakasimba pasi pechisimba kuti uwane zvakananga zvikamu kana zvisipo. Iine zvakanakira yakakwira yekushandisa mwero simbi yemvura, yakareruka maitiro uye yakasimba mhando. Isimbi-inoponesa simbi inogadzira tekinoroji ine mikana yekushandisa yekushandisa.
- Direct svina kukanda: pfapfaidzo pendi, kukanda chiwanikwa, pedyo muforoma, kumanikidza, bata kumanikidza, kuburitsa kumanikidza, kupatsanurwa muforoma, demold isina chinhu, itangezve;
- Yakananga Svina kukanda: pfapfaidzo unhani, muforoma clamping, kudyisa, kuzadza, kumanikidza, kumanikidza kubata, kumanikidzwa zororo, kutsemuka kweforoma, isina demolding, kugadzirisa patsva.
Unyanzvi zvikamu:
- Iyo inogona kubvisa kukanganisa kwemukati senge pores, shrinkage maburi uye shrinkage porosity;
- Yakadzika pamusoro pekuomarara uye yakanyanya kujeka kurongeka;
- Inogona kudzivirira kuitika kwekukanda kutsemuka;
- Zviri nyore kuziva michina uye otomatiki.
Kushanda: Inogona kushandiswa kuburitsa dzakasiyana mhando alloys, senge aruminiyamu chiwanikwa, zinc chiwanikwa, mhangura chiwanikwa, ductile simbi, nezvimwewo.
9.Lost Foam Kukanda
Yakarasika furo kukanda (inozivikanwa zvakare seyakazara muforoma kukanda): Iko kusanganisa parafini wakisi kana furo modhi ane saizi yakafanana uye chimiro kune iyo castings kuti vagadzire masumbu. Mushure mekutsvaira nekuomesa zvipfeko zvinokatyamadza, ivo vanovigwa mujecha rakaoma re quartz yeiyo vibration modelling. Iyo mhando nyowani yekukanda nzira iyo iyo furu iri vaporized nekudururira pasi pekumanikidzwa, iyo simbi yemvura inotora chinzvimbo chehuvhu, uye iyo yekukanda inoumbwa mushure mekusimbiswa uye kutonhora.
Maitiro ekuyerera: pre-achipupira furo → furo → kunyorova → kuomesa → modelling → kudira → kudonha → kuchenesa
Unyanzvi zvikamu:
- Kudzingwa kune kukwirira kwakaringana uye hakuna jecha moyo, iyo inoderedza nguva yekugadzirisa;
- Hapana nzvimbo yekuparadzanisa, dhizaini dhizaini uye yakakwira rusununguko;
- Kugadzira kwakachena, hapana kusvibiswa;
- Deredza mari yekudyara neyekugadzira.
Kushanda: Iyo inokodzera kugadzirwa kwemanyoro castings ehukuru hwakasiyana nezvivakwa zvakaomarara, mhando dzisingagumi alloys, uye zvisingagumi mabhureki ekugadzira. Senge grey kukanda simbi injini bhokisi, yakakwira manganese simbi kugokora, nezvimwe.
10.Continual Kukanda
Kuenderera mberi kwekukanda: Iyo yepamusoro nzira yekukanda. Musimboti wayo ndeyekuenderera uchidururira simbi yakanyungudutswa mune yakakosha simbi muforoma inonzi muforoma Iyo yakasimbiswa (yakakora) castings inoenderera ichibviswa kubva muforoma. Dhonza mugumo mumwe, unogona kuwana chero hurefu kana yakatarwa kureba kukanda.
Inoenderera Kukanda Maitiro:
Unyanzvi zvikamu:
- Nekuda kwekukurumidza kutonhodza kwesimbi, iyo kristaro yakaoma, chimiro chiri yunifomu, uye michina zvivakwa zviri nani;
- Sevha simbi uye wedzera goho;
- Maitiro acho akareruka, uye kuenzanisira uye mamwe maitiro anobviswa, nekudaro kudzikisira kusimba kwevashandi; nzvimbo inodiwa yekugadzira inoderedzwawo zvakanyanya;
- Kuenderera mberi kwekukanda kugadzirwa kuri nyore kuona michina uye otomatiki, uye kunatsiridza kugadzirwa kwekuita.
Kushanda: Kuenderera mberi kwekukanda kunogona kushandiswa kukanda simbi, simbi, alloys emhangura, aluminium alloys, magnesium alloys uye mamwe marefu castings ane anogara achiyambuka-echikamu maumbirwo, senge ingots, slabs, billets, machubhu, nezvimwe.
Ndokumbirawo uchengete kwainobva nekero yechinyorwa chino kuti iprote zvakare:Mhando Gumi Kukanda Maitiro MuForeries
Minghe Kambani Inokanda Kambani dzakatsaurirwa kugadzira uye kupa mhando uye epamusoro kuita Kukanda Zvikamu (simbi kufa zvikamu zvekukanda mhando zvinonyanya kusanganisira Mutete-Wall Yakakanda Kukanda,Hot Chamber Die Kukanda,Cold Chamber Die Kukanda), Round Sevhisi (Die Kukanda Service,Cnc machine,Kugadzira Mould, Surface Kurapa) .Chero tsika yeAluminium kufa kukanda, magnesium kana Zamak / zinc kufa kukanda uye zvimwe zvinodiwa zvekukanda zvinogamuchirwa kuti utibate.
Pasi pekutonga kwe ISO9001 uye TS 16949, Maitiro ese anoitwa kuburikidza nemazana epamberi kufa michina yekukanda, mishina-axis michina, uye zvimwe zvivakwa, zvinobva kumablasters kusvika ku Ultra Sonic yekuwachisa michina. timu yevainjiniya vane ruzivo, vashandisi uye vaongorori kuti zvigadzirwa zvemutengi zviitike.
Chibvumirano chinogadzira kufa kwekufa. Unyanzvi hunosanganisira inotonhorera kamuri aluminium kufa kukanda zvikamu kubva pa0.15 lbs. kusvika ku6 lbs., kukurumidza shanduko kumisikidzwa, uye machining. Kukosha-kwakawedzerwa masevhisi anosanganisira kukwiza, kudedera, kuita deburring, kupfura kupfura, kupenda, kupenda, kupfeka, kuungana, uye kushandisa. Zvishandiso zvakashanda pamwe zvinosanganisira alloys senge 360, 380, 383, uye 413.
Zinc kufa kukanda dhizaini rubatsiro / panguva imwe chete mabasa einjiniya. Tsika inogadzira chaiyo zinc kufa castings. Miniature castings, yakanyanya kumanikidza kufa castings, yakawanda-slide muforoma castings, yakajairwa muforoma castings, yuniti kufa uye yakazvimirira kufa castings uye mhango yakavharwa castings inogona kugadzirwa. Castings inogona kugadzirwa muhurefu uye hupamhi kusvika makumi maviri nemana mukati. Mu +/- 24 mukati. Shiviriro.
ISO 9001: 2015 yakasimbiswa inogadzira kufa cast magnesium, Kugona kunosanganisira yakakwira-yekumanikidza magnesium kufa kukanda kusvika 200 ton inopisa kamuri & 3000 toni kamuri inotonhorera, dhizaini dhizaini, kupora, kuumba, kugadzira, poda & pendi yemvura, yakazara QA ine CMM kugona , gungano, kurongedza & kuendesa.
ITAF16949 yakasimbiswa. Kuwedzera Kukanda Sevhisi Sanganisira utsvaga kukanda,jecha kukanda,Gravity Kukanda, Yakarasika Furo Kukanda,Kukanda kweCentrifugal,Vacuum Kukanda,Permanent Mould KukandaUnyanzvi hunosanganisira EDI, rubatsiro rweinjiniya, yakasimba modelling uye yechipiri kugadzirisa.
Kukanda Maindasitiri Zvikamu Nyaya Dzedzidzo dze: Mota, Mabhasikoro, Ndege, Zvimhanzi, Watercraft, Optical zvishandiso, Sensors, Models, Zvigadzirwa zvemagetsi, Mahombekombe, Mawachi, Michina, Injini, Furniture, Zvishongo, Jigs, Telecom, Mheni, Midziyo yekurapa, Mifananidzo yemifananidzo, Marobhoti, Zvivezwa, Zvishandiso zveruzha, Zvekushandisa zvemitambo, Matombo, Matoyi nezvimwe.
Chii chatinogona kukubatsira iwe kuti uite zvinotevera?
∇ Enda Kune Homepage Ye Die Kukanda China
→Kukanda Zvikamu-Tsvaga zvatakaita.
→ Ralated Matipi Nezve Vanofa Vanokanda Services
By Minghe Die Kukanda Mugadziri | Categories: Zvinyorwa Zvinobatsira |zvinhu Tags: Aluminium Casting, Zinc Kukanda, Magnesium Kukanda, Titanium Kukanda, Stainless Simbi Kukanda, Brass Kukanda,Bronze Kukanda,Kukanda Vhidhiyo,History History,Aluminium Die Casting | Comments Off