Iyo Kudzora Kwakafa Kudzingwa Maitiro
Nekuda kwekusiyana kwezvinhu zvinokanganisa mhando yekukanda uye kuomarara kwemaitiro ekugadzira, parizvino zvine hungwaru sangano, kutonga maitiro kune basa rakakosha mukusimudzira dhizaini dhizaini, dzidziso yehunyanzvi uye kudzora kwekugadzira, nechinangwa chekupedzisira kuve kuziva kudzivirira kwakaringana uye kugadzirisa kwekukanganisa kuremara. Kuongorora kupfupisa nezve chiwanikwa chinonyunguduka kudzora, chakuvhuvhu uye kufa-kukanda maitiro ekudzora, mukati nekunze kuongororwa kwezvigadzirwa kunoitwa.
Dhizaini yeinjini block inovandudza munzira yekureruka uye kuomarara. Nekuda kweiyo yakaderera density uye yakanaka kurasa mashandiro, aluminium alloy inowanzo shandiswa kugadzira aerospace uye auto zvikamu zvine yakaoma maumbirwo, matete masvingo, uye epakati mitoro. Akateedzana einjini mabhuroko anogadzirwa neChangan Mota Jiangbei Injini Fekitori inoumbwa neakakwira-kumanikidza kukanda muforoma ine yemhando yepamusoro aruminiyamu chiwanikwa (chakafanana neyechipfuyo brand YL113). Iyo cylinder block yeiyi inoteedzana enjini ndeye yakasimba-yakasimba, yakatetepa-yakakomberedzwa yakaoma kukanda. Mazhinji emakomba ari pane humburumbira anovharirwa neakaumbwa macustoms, ayo asingori chete nezvinodiwa zvepamusoro zvemuchina semidziyo uye michina yekufa, asi kutonga kwese kugadzirwa kunovimbisa kuendesa Iyo kutenderera iri mushe, uye iko kuvandudzwa kwehunhu hwechigadzirwa zvakare kune kwakakosha kukosha.
Maitiro Ekutonga
Mukuita manejimendi manejimendi yekufa-yekukanda kugadzirwa, zvinonyanya kukosha kudzikamisa nekuvandudza mhando yechigadzirwa kubva kumatunhu ealuminium emvura kudzora, chakuvhuvhu kudzora, kufa-kukanda maitiro kutonga uye chigadzirwa kuongorora.
Aluminium Mvura Kudzora
Iyo solidification kuremara kwe cast aluminium alloy yakakanganisa zvakanyanya mashandiro eanokandwa, uye kudzora kana kubviswa kwe solidification kuremara kwakakosha zvikuru kugadzirisa goho re castings. Sezvo zvinodikanwa zveiyo yakazara zvivakwa zvealloys zviri kuramba zvichikwira uye zvichikwira,
Tsvagiridzo yekuwedzera mamwe marudzi ezvekutsikisa zvinhu kuti ivandudze zvivakwa zvealloys zvave kuwedzera uye zvakadzama, uye nzira yealloy yekugadzirisa kudzora yave kunyanya kukosha. Zvakajairika solidification zvikanganiso mu cast aluminium alloys muinjiniya, senge kusarura, kupisa kupisa, microporosity, shrinkage, nezvimwe, zvinoda kudzorwa kubva kunobva. Mukupindura kugadzirwa kwemavara, hwaro hwekugadzira iyi modhi paChangan Automobile yeJiangbei Injini Yekutengesa inotora yakananga kuunzwa kwealuminium yakanyungudutswa, saka hunhu hwekunongedzera kwakananga kwealuminium yakanyungudika inoshandiswa sehwaro hwekuti iyo aluminiyamu yakanyungudika inosangana nezvinodiwa. Iyo yekugezesa sampuro yekugadzirira chishandiso inoshandiswa kuona iyo density yakaenzana yealuminium alloy ingots, iyo spectrum analyzer inoshandiswa pakuongorora kwemuviri uye kwemakemikari, uye K -mhando yekutsvaga inoitwa pamushini-padivi furimi aluminium mvura nguva dzose yekutarisa kuwanda zvakaenzana, makemikari kuumbwa, uye kuchena kwealuminium alloy.
Kudzora Mould
Iwo manejimendi, kuongorora gwapa, uye kugadzirisa kweforoma chikamu chekufa-kukanda, uye chimiro cheforoma chakakosha kune chigadzirwa mhando. Iyo chigadziko cheforoma chakagadzirwa nesimbi yakakandwa. Munguva yejekiseni, iyo aluminium mvura inoyerera ichipinda mukamuri yekumanikidza, iyo sprue, muchinjikwa mumhanyi, uye yemukati inomhanya yejekiseni kuumba kubva pasi kusvika kumusoro. Iyo yese gating system ndeye yakavharwa dhizaini yekudzikisa iyo aluminium mvura yekupinda. Iko mukati meforoma mhango inovhurwa nemvura kuenzanisa tembiricha munda weforoma, uye mativi ese esirinda muviri anosimbiswa panguva imwe chete, uye gasi rinosara riri mumvura yealuminium rinoparadzirwa nekuparadzirwa. Nepose pazvinogona napo, maburi ekukanda anofanirwa kuve akaumbirwa nemvura inotonhorera. Iyo yakanyanya-kumanikidza poindi kutonhora kana kudzosera nzira yekutonhora yemvura inogona kusarudzwa zvinoenderana nezvinodiwa chaiko. Mvura inotonhora inogona kusvika kumusoro kwepini yekukanda, kuitira kuti chikamu chepamusoro chigone kutonhodzwa.
Mukugadzirwa kwemaitiro, tembiricha yekuumbisa ine pesvedzero huru pane chigadzirwa uye nehupenyu hweforoma, uye tembiricha yakakwira inonamira kuomerera, pamusoro pekukanda kwakaomarara, uye maburi ekuderera uye kutsemuka kunogona kuitika. Nekuda kwekunamatira kweforoma, iko kukweshera.
Iko kuwedzera kwekukwesana kunowedzera simba remuno rakasimba, izvo zvinoita kuti kufamba kwenzvimbo yacho kuumbike uye kukuvadza muforoma. Mould tembiricha kudzora inowanzo gadzirirwa maererano nemadziro pakukora kwekukanda uye kugoverwa kwesimbi yakanyungudutswa. Iyo inotonhorera mvura vhoriyamu uye nguva inotonhorera yemativi akasiyana eiyo mold inogona kugadziridzwa. Kutonhora kunze kweforoma kwakakoshawo, uye ine zvakawanda zvekuita nechinzvimbo, nhungamiro nemaitiro (nguva) yemusununguri wekumwaya. Iko kusarudzwa, chiyero uye huwandu hweanosunungura mumiririri kuchachinja mashandisirwo eforoma uye mhando yechigadzirwa. Kugadziriswa kweMold kwakakamurwa kuita kudzivirira kwekuchengetedza, kufungidzira kwekuchengetedza uye kuongorora nzvimbo. Sarudza inodzivirira yekuchengetedza kutenderera kweiyo furu zvinoenderana neruzivo rwakaunganidzwa, sarudza yekufungidzira yekuchengetedza nguva zvinoenderana nehurumende uye kushandiswa kweforoma, uye kuita ongororo yezuva nezuva panguva yekugadzirwa. Iyo yekuchengetedza yezvinyorwa inovhara kutonhodza system (mvura, mafuta, gasi), vharuvhu system, kuiswa chisimbiso, kuchenesa kwevhu pamusoro, nezvimwe.
Maitiro Parameter Kudzora
The kuzvidzora uye Optimization pamusoro vanofa-vachikanda muitiro chinhu chinokosha chikamu vanofa-Kudzingwa kugadzirwa, izvo zvinokanganisa zvakananga pamusoro uye womukati unhu kufa-vachikanda zvikamu. Iyo parameter yefa yekukanda maitiro kunyanya inosanganisira kumanikidza, kumhanya uye nguva.
Iwo technical technical parameter anochengetedzwa zvakawandisa kuona kuti kuyerera, kusimbisa, uye kupisa kupisa kwesimbi yemvura inoitwa nenzira yakatarwa, kuitira kuona mhando yezvikamu zvekufa. Iyo yemukati mhando yekukanda inonyatso kunetsekana neshanduko yeiyo jekiseni paramita. Kana iko kumanikidza kwakanyanya kuderera, kuraswa kunenge kune akawanda pores, shrinkage uye zvimwe zvinokanganisa. Kana iko kumanikidza kwakanyanya, kunyangwe chimiro chekukanda chakakora, chinoburitsa kupenya kukuru uye mabhureki, izvo zvinokanganisa furu. . Munguva yekugadzira, zvakakoshawo kuratidza kuti shanduko poindi kubva kunonoka kuenda kukurumidza jekiseni yakakosha zvakare. Kuti ishanduke nguva isati yakwana, iyo yakaumbwa nesimbi yakanyungudika inopfuura nemumhanyi wemukati uye inopinda mudumbu nepamhanyisa. Iyo nzira ndeyakareba, ichikonzera kusagadzikana kwekuyerera kwealuminium yakanyungudutswa, inosanganisira yakawanda gasi, uye zviri nyore kuumba zvimwe zvisirizvo Kukanda zvikanganiso; yakanyanyisa kunonoka kuti ishanduke, iyo aruminiyamu mvura inogara mukamuri yekumanikidza kwenguva yakareba, iyo tembiricha yakadzika, zviri nyore kuburitsa zvinotonhora, kudira kwakakwana uye zvimwe zvinokanganisa. Muchokwadi, kubva pakuona kwemaatomical maonero, kuvepo kwe pores uye shrinkage maburi mukukanda hakudzivisike. Chinokosha ndechekugadzirisa majekiseni ejekiseni kuitira kuti gasi iri mune aruminiyamu mvura igone kuburitswa zvinobudirira sezvazvinogona, uye iyo shoma shoma yasara ye pores inoparadzirwa uye inoparadzirwa mukati. Kupinda muchikamu kunokonzeresa kuburitsa kwekukanda. Iyo yekumhanya jekiseni inosanganisira iyo punch kumhanya (ndokuti, kumhanya kwekumhanyisa kwepistoni mujekiseni rejekiseni) uye kumhanya kwekuzadza (ndokuti, kumhanya kwepashure).
Kuzadza kumhanya kunoreva kumhanyisa kumhanya kwesimbi yakanyungudika ichipfuura nemumhanyi wemukati, inova paramende yakakosha yekuona mhando yeanofa kufa. Iyo jekiseni nguva inoumbwa neinononoka jekiseni nguva, yekukurumidza jekiseni nguva, nguva yekumanikidza, kumanikidza kubata nguva, uye nguva yekuchengetedza nguva. Mukugadzirwa, iyo inobata nguva uye chakuvhuvhu chengetedzo nguva inowanzo kudzorwa uye kukwidziridzwa pamwe chete, kunzi sekubata kumanikidza uye nguva yekuchengetedza nguva. Inokwana kubata kumanikidza uye chakuvhuvhu chengetedzo nguva zvinoreva kuti kufa kuraswa hakukanganise kana kutambanudza panguva yeforoma kuvhura uye ejection. Mamiriro anodikanwa ekupaza. Aya parameter akakosha anoda kuongororwa zuva nezuva uye nekuenderera mberi achigadziridzwa zvinoenderana nemamiriro ekukanda.
Chigadzirwa Kuongorora
Kuongorora kukanda kunosanganisira kutaridzika uye kuongorora saizi, zvemukati zvemhando yekuongorora, pre-cast gomba nzvimbo yekutarisa, rusvingo ukobvu kuongorora, humburumbira liner madziro ukobvu mutsauko kuongorora, kukanda kupisa kurapwa isina internet yekupedzisira kuongorora, zvinoenderana nehurongwa hwevashandi uye chaicho kugadzirwa zvinodiwa zvinoenderana yakatarwa frequency uye mureza Kukanda kunokodzera.
Sampling kuongororwa mune yekugadzira maitiro kunogona kuona matambudziko nekufamba kwenguva uye kuita nekukurumidza, uye hakuzokonzere batch matambudziko nekuda kwekusagadzikana kwenguva kwekuwanikwa kwedambudziko.
sutras
Kufa-kukanda kugadzirwa inguva yakaoma kuita, inosanganisira mhando yesimbi yakanyungudutswa, mamiriro eakafa-achikanda muforoma, iwo marita emuchina wekufa-wekukanda, iyo yekufa-yekurasa maitiro uye chigadzirwa kuongorora, nezvimwe. zvakabatana zvakanyanya nemhando yezvikamu zvekufa-zvichikandwa. Mukufa-kwekukanda kugadzirwa, maitiro anosarudza mhedzisiro, yakanaka maitiro manejimendi inotungamira kune yakagadzika chigadzirwa mhando, uye inodzorwa kuwanda kugadzirwa kunounza hukuru-hukuru hupfumi mabhenefiti.
Ndokumbirawo uchengete kwainobva nekero yechinyorwa chino kuti iprote zvakare: Iyo Kudzora Kwakafa Kudzingwa Maitiro
Minghe Kambani Inokanda Kambani dzakatsaurirwa kugadzira uye kupa mhando uye epamusoro kuita Kukanda Zvikamu (simbi kufa zvikamu zvekukanda mhando zvinonyanya kusanganisira Mutete-Wall Yakakanda Kukanda,Hot Chamber Die Kukanda,Cold Chamber Die Kukanda), Round Sevhisi (Die Kukanda Service,Cnc machine,Kugadzira Mould, Surface Kurapa) .Chero tsika yeAluminium kufa kukanda, magnesium kana Zamak / zinc kufa kukanda uye zvimwe zvinodiwa zvekukanda zvinogamuchirwa kuti utibate.
Pasi pekutonga kwe ISO9001 uye TS 16949, Maitiro ese anoitwa kuburikidza nemazana epamberi kufa michina yekukanda, mishina-axis michina, uye zvimwe zvivakwa, zvinobva kumablasters kusvika ku Ultra Sonic yekuwachisa michina. timu yevainjiniya vane ruzivo, vashandisi uye vaongorori kuti zvigadzirwa zvemutengi zviitike.
Chibvumirano chinogadzira kufa kwekufa. Unyanzvi hunosanganisira inotonhorera kamuri aluminium kufa kukanda zvikamu kubva pa0.15 lbs. kusvika ku6 lbs., kukurumidza shanduko kumisikidzwa, uye machining. Kukosha-kwakawedzerwa masevhisi anosanganisira kukwiza, kudedera, kuita deburring, kupfura kupfura, kupenda, kupenda, kupfeka, kuungana, uye kushandisa. Zvishandiso zvakashanda pamwe zvinosanganisira alloys senge 360, 380, 383, uye 413.
Zinc kufa kukanda dhizaini rubatsiro / panguva imwe chete mabasa einjiniya. Tsika inogadzira chaiyo zinc kufa castings. Miniature castings, yakanyanya kumanikidza kufa castings, yakawanda-slide muforoma castings, yakajairwa muforoma castings, yuniti kufa uye yakazvimirira kufa castings uye mhango yakavharwa castings inogona kugadzirwa. Castings inogona kugadzirwa muhurefu uye hupamhi kusvika makumi maviri nemana mukati. Mu +/- 24 mukati. Shiviriro.
ISO 9001: 2015 yakasimbiswa inogadzira kufa cast magnesium, Kugona kunosanganisira yakakwira-yekumanikidza magnesium kufa kukanda kusvika 200 ton inopisa kamuri & 3000 toni kamuri inotonhorera, dhizaini dhizaini, kupora, kuumba, kugadzira, poda & pendi yemvura, yakazara QA ine CMM kugona , gungano, kurongedza & kuendesa.
ITAF16949 yakasimbiswa. Kuwedzera Kukanda Sevhisi Sanganisira utsvaga kukanda,jecha kukanda,Gravity Kukanda, Yakarasika Furo Kukanda,Kukanda kweCentrifugal,Vacuum Kukanda,Permanent Mould KukandaUnyanzvi hunosanganisira EDI, rubatsiro rweinjiniya, yakasimba modelling uye yechipiri kugadzirisa.
Kukanda Maindasitiri Zvikamu Nyaya Dzedzidzo dze: Mota, Mabhasikoro, Ndege, Zvimhanzi, Watercraft, Optical zvishandiso, Sensors, Models, Zvigadzirwa zvemagetsi, Mahombekombe, Mawachi, Michina, Injini, Furniture, Zvishongo, Jigs, Telecom, Mheni, Midziyo yekurapa, Mifananidzo yemifananidzo, Marobhoti, Zvivezwa, Zvishandiso zveruzha, Zvekushandisa zvemitambo, Matombo, Matoyi nezvimwe.
Chii chatinogona kukubatsira iwe kuti uite zvinotevera?
∇ Enda Kune Homepage Ye Die Kukanda China
→Kukanda Zvikamu-Tsvaga zvatakaita.
→ Ralated Matipi Nezve Vanofa Vanokanda Services
By Minghe Die Kukanda Mugadziri | Categories: Zvinyorwa Zvinobatsira |zvinhu Tags: Aluminium Casting, Zinc Kukanda, Magnesium Kukanda, Titanium Kukanda, Stainless Simbi Kukanda, Brass Kukanda,Bronze Kukanda,Kukanda Vhidhiyo,History History,Aluminium Die Casting | Comments Off